What is the difference between 316 and 316L? Stop being clueless about it!

 

We all know that 316L is a grade of stainless steel; AISI 316L is the corresponding American designation, and SUS 316L is the Japanese equivalent. The Chinese standard designation is 022Cr17Ni12Mo2 (new standard), while the old designation was 00Cr17Ni14Mo2; these indicate the primary presence of Cr, Ni, and Mo, with the numbers representing their approximate percentages.
So, do you know the difference between 316 and 316L?

First, let's look at the chemical composition of the materials.
[Image]
We can see that the carbon content differs: 316L has a lower carbon content, resulting in superior corrosion resistance. Here, the "L" stands for "Low."
To put it in simple, everyday terms: if everyone considers a clean, minimalist look stylish, but you sport a wild, garish "Shamate" hairstyle, then you are "low" (uncool/tacky).
If everyone is discussing Shakespeare, but you insist on talking about Zhao Benshan, then you are "low."

If your friends love the arts-music, chess, poetry, and painting-but you prefer playing mahjong with the neighborhood aunties, then you are "low."
If everyone values ​​cleanliness and hygiene, but you spit and litter everywhere, then you are "low."

In English, "low" means... well, low. Now you understand the difference! Do you also know the differences between 304 and 304L, or 317 and 317L?
1. Welding Methods
Since the work typically involves stainless steel piping of various sizes, and given the welding characteristics of stainless steel-specifically the need to minimize heat input-two methods are employed: manual arc welding and argon arc welding (TIG welding).
For pipe diameters larger than 159 mm, argon arc welding is used for the root pass, and manual arc welding is used for the capping pass. For pipe diameters smaller than 159 mm, argon arc welding is used exclusively. The welding equipment used is the WS7-400 inverter arc welder, which supports both manual arc and argon arc welding. 2. Welding Materials
Austenitic stainless steel is a material with special properties; to ensure the welded joint possesses matching characteristics, the "matching composition" principle is followed when selecting welding materials. Additionally, to enhance the joint's resistance to hot cracking and intergranular corrosion by promoting the formation of a small amount of ferrite within the weld, H00Cr19Ni12Mo2 argon arc welding wire and CHSO22 manual arc welding electrodes are selected as filler materials. Their chemical compositions are listed in Tables 1 and 2.
[Image]

3. Welding Parameters
A key characteristic of austenitic stainless steel is its sensitivity to overheating; therefore, low-current, high-speed welding techniques are employed. For multi-pass welding, the interpass temperature must be strictly controlled and kept below 60°C. Specific parameters are detailed in Table 3.
[Image]

4. Groove Design and Assembly Tack Welding
A V-shaped groove design is adopted. Due to the use of lower welding currents resulting in shallower penetration, the groove root face is smaller than that used for carbon steel (approximately 0–0.5 mm), while the groove angle is larger (approximately 65°–70°). The configuration is shown in Figure 1.
[Image]
Stainless steel has a high coefficient of thermal expansion, leading to significant welding stresses; consequently, strict tack welding procedures are required. Two-point tacking is used for pipes with a diameter (d) ≤ Φ89 mm, three-point tacking for d = Φ89–Φ219 mm, and four-point tacking for d ≥ Φ219 mm. The length of each tack weld is 6–8 mm. 5. Welding Technical Requirements
① For manual arc welding, use DC reverse polarity (DCEP); for argon arc welding (TIG), use DC straight polarity (DCEN).


② Before welding, remove surface oxide scale from the welding wire using a stainless steel wire brush and clean it with acetone; dry welding electrodes at 200–250°C for 1 hour and use them immediately after removal from the oven.
③ Before welding, clean off oil and other contaminants within a 25mm range on both sides of the joint bevel, and clean this 25mm area with acetone.
④ For argon arc welding, use a nozzle diameter of Φ2mm and a ceriated tungsten electrode with a diameter of Φ2.0mm.
⑤ When welding stainless steel using argon arc welding, argon gas shielding must be applied to the backside to ensure proper root bead formation. Use a localized internal argon purging method with a flow rate of 5–14 L/min; the external (torch-side) argon flow rate should be 12–13 L/min.
Note
① During root pass welding, keep the weld bead as thin as possible while ensuring good fusion with the root face; shape the crater into a gentle slope at the end of the weld, and grind away any shrinkage cavities. Arc striking and extinguishing must occur within the bevel; fill the crater completely when extinguishing the arc to prevent crater cracks.

② Since this material is austenitic stainless steel, strictly control the interpass temperature and post-weld cooling rate to prevent carbide precipitation (sensitization) and intergranular corrosion. Maintain the interpass temperature below 60°C, perform immediate water cooling after welding, and use a segmented welding sequence. Refer to Figure 2 for the specific segmentation method. This symmetrical, dispersed welding sequence increases the joint's cooling rate and reduces welding stress.
Image

info-809-338
6. Results
① Visual inspection revealed no defects such as porosity, weld spatter/nodules, depressions, or undercut; the weld profile was well-formed.
② Tensile and bending tests performed on the specimens showed that all mechanical property indicators met requirements; no defects such as lack of fusion or cracks were found.
③ Macroscopic metallographic examination showed good fusion of the weld bead, with a penetration depth of 1–1.5 mm. Microscopic metallographic examination revealed a fully austenitic microstructure in both the base metal and the heat-affected zone, while the weld metal exhibited an austenite-plus-ferrite (4%) structure; these characteristics fully meet the requirements for resistance to intergranular corrosion and embrittlement, ensuring the quality of the welding work during on-site construction by the Coal Chemical Company.

 

 

 