Oct 08, 2023 Leave a message

Thin-wall Injection Molding Is Difficult, Here Is A List Of Common Problems! ·

 

Thin-wall injection molding is mainly used in:

According to research, thin-wall injection molding is currently widely used in food containers, medical boxes, cosmetics, stationery and even multimedia packaging in China. For example: disposable packaging boxes, cosmetic bottles and other daily necessities.

1. What is thin-wall injection molding?

Thin-wall injection molding technology is also called thin-wall plastic parts injection molding technology. There are three definitions:

The ratio of flow length to thickness L/T, that is, the ratio of the flow length L from the melt entering the mold to the farthest point of the cavity where the melt must be filled and the corresponding average wall thickness T is 100 or 150 or more, which is thin-walled injection molding. ;

Injection molding method where the thickness of the molded plastic part is less than 1 mm and the projected area of the plastic part is more than 50 c㎡;

Injection molding where the wall thickness of the molded plastic part is less than 1 mm (or 1.5mm), or t/d (plastic part thickness t, plastic part diameter d, for disc-shaped plastic parts) below 0.05 is defined as thin-wall injection molding .

It can be seen that the critical value defined for thin-wall injection molding will also change, and it should be a relative concept.

2. Selection of raw materials

Requirements for raw materials: large flow length, high impact strength, high thermal distortion temperature, high thermal stability, low directionality and good dimensional stability; also consider the low-temperature impact rigidity, flame retardancy, mechanical assembly and appearance of the plastic raw materials Quality etc.

Currently commonly used thin-wall injection molding raw materials include: polycarbonate (PC), acrylonitrile-butadiene-styrene (ABS), PC/ABS blends and PA6, etc. As wall thickness decreases, plastics with better physical properties are needed to maintain part strength.

Thin-wall injection molding technology is also called thin-wall plastic parts injection molding technology.

There are three definitions:

One: the ratio of flow length to thickness L/T, that is, the ratio of the flow length L from the melt entering the mold to the farthest point of the cavity where the melt must be filled and the corresponding average wall thickness T is 100 or 150 or more for injection molding. Thin wall injection molding;

Second: Injection molding method where the thickness of the molded plastic part is less than 1 mm and the projected area of the plastic part is more than 50 c㎡;

Third: Injection molding with a wall thickness of less than 1 mm (or 1.5mm), or t/d (plastic part thickness t, plastic part diameter d, for disc-shaped plastic parts) below 0.05 is defined as thin. Wall injection molding.

It can be seen that the critical value defined for thin-wall injection molding will also change, and it should be a relative concept.

Second, the selection of raw materials requires raw materials: large flow length, high impact strength, high thermal deformation temperature, high thermal stability, low directionality and good dimensional stability; the low-temperature impact rigidity, flame retardancy, and mechanical properties of the plastic raw materials must also be considered. Assemblability and appearance quality, etc.

Currently commonly used thin-wall injection molding raw materials include: polycarbonate (PC), acrylonitrile-butadiene-styrene (ABS), PC/ABS blends and PA6, etc. As wall thickness decreases, plastics with better physical properties are needed to maintain part strength.

Analysis of Three Common Defects Although thin-walled plastic parts have many advantages, it reduces the formability of plastic parts, making it impossible to form these thin-walled plastic parts using conventional injection molding methods. When molding thin-walled plastic parts, there are the following common problems:

 

1. Short shot

Short shot refers to the quality defect of incomplete plastic parts caused by incomplete filling of the mold cavity, that is, the melt has solidified before filling is completed.

The filling and cooling processes of conventional injection molding are intertwined. When the polymer melt flows, the melt front encounters the relatively low-temperature core surface or cavity wall, and a condensation layer is formed on its surface. The melt continues to flow forward in the condensation layer. As the thickness of the condensation layer increases, the actual cavity flow channel becomes narrower. The thickness of the condensation layer has a significant impact on the flow of the polymer. Because the thickness of the plastic part is relatively thick during conventional injection molding, the impact of the condensation layer on injection molding is not great at this time. However, in thin-wall injection molding, when the ratio of the thickness of the condensation layer to the thickness of the plastic part gradually increases as the thickness of the plastic part becomes thinner, this effect will be great. Especially when the sizes of the two can be compared with each other.

When the thickness of the plastic part decreases, the influence of the condensation layer on the flow will increase exponentially, which also illustrates the great influence of the condensation layer in thin-wall injection molding. If we only consider injection molding, the injection molding machine needs to have a high injection rate so that the rate at which the plastic melt fills the cavity exceeds the growth rate of the condensation layer (or the growth rate of the condensation layer is slowed down), so that the flow section can be Complete the filling action before closing and perform injection molding of thin-walled plastic parts.

When the flow length is 300mm and the wall thickness of the plastic part is 3.0 mm, L/T is 100, which is easily achieved using conventional injection molding technology; but when the wall thickness of the plastic part drops below 1.0mm, this was once easy Achieved flow length to thickness ratio (100) becomes very difficult to achieve.


2. Warping deformation

Warpage deformation is a defect in plastic parts caused by uneven internal stress. The causes of warpage deformation are uneven shrinkage, uneven orientation and uneven cooling.

☞ Improvement method: The warpage deformation defects of plastic parts can be improved by balancing the cooling system, adjusting cooling time, holding pressure and holding time.


3. Welding line

The weld line is the boundary formed when two or more melt flow fronts in the cavity fuse. Stress concentration is easy to occur at the welding line, which weakens the mechanical strength of the plastic part, which is particularly detrimental to the mechanical properties of the plastic part, especially the thin-walled plastic part. The plastic part is very easy to crack at the welding line after being subjected to external force.

☞ Improvement method: During design, the location of the weld line can be reduced or changed by reducing the number of gates or changing the location of the gates to meet the design requirements of the plastic part.


4. Shortage of materials

The small parts and corners of the finished product cannot be completely formed because the mold is not processed in place or the exhaust is not smooth, and the molding is due to insufficient injection dose or pressure, etc., resulting in design defects (insufficient flesh thickness).

☞ Improvement methods: Correct the mold where the material is lacking, take or improve exhaust measures, increase the thickness of the meat, improve the gate (increase the gate, increase the gate), increase the injection dose, increase the injection pressure and other measures to improve.


5. Shrink

It often occurs where the wall or flesh thickness of the molded product is uneven, due to differences in the cooling or solidification shrinkage of hot-melt plastics. For example, steal the meat from the back of the ribs, the edges with side walls, and the back of the BOSS pillar, but keep at least 2/3 of the meat thickness.

☞ Improvement methods: Improvements can be made by thickening the flow channel, enlarging the gate, adding exhaust, increasing the material temperature, increasing the injection pressure, and extending the pressure holding time.


6. Surface image

It often occurs on the back side of BOSS pillars or ribs that have been stripped of flesh, or the stress marks are reduced due to excessively high design of the core or ejector pin.

☞ Improvement method: It can be corrected by modifying the core, ejector pin, sandblasting of the master mold surface, etc., and adopting methods such as reducing the brightness of the mold surface, lowering the injection speed, and reducing the injection pressure.


7. Qi patterns

It occurs at the gate, mostly because the mold temperature is not high, the injection speed and pressure are too high, the gate is improperly set, and the plastic hits the spoiler structure during pouring.

☞ Improvement methods: changing the gate, polishing the runner, enlarging the cold material area of ​​the runner, enlarging the gate, adding texture to the surface (can also be done by adjusting the machine or repairing the mold to catch up with the joining line), raising the Solve the problem by reducing the mold temperature, reducing the injection speed, and reducing the injection pressure.


8. Joining line

It occurs at the intersection of two material flows, such as the intersection of material flows from two inlets and the intersection of material flows bypassing the core. It is caused by a drop in material temperature and poor exhaust.

☞ Improvement methods: You can change the inlet gate, add a cooling well, open an exhaust slot or nip the male mold surface, etc. You can also increase the material temperature, increase the mold temperature, etc.


9. burrs

The joint between the male and female molds often occurs due to poor mold clamping, improper processing of mold surface corners, insufficient clamping force during molding, excessive material temperature and pressure, etc.

☞ Improvement methods: You can modify the mold, re-close the mold, increase the clamping force, lower the material temperature, reduce the injection pressure, reduce the holding time, reduce the holding pressure, etc.


10. Deformation

Slender parts, thin-walled parts with large areas, or larger finished products with asymmetric structures are caused by uneven cooling stress or uneven ejection force during molding.

☞Improvement method: You can correct the ejector pin, set up a pull pin for tensioning, etc. If necessary, add nip to the male mold to adjust the deformation, adjust the mold temperature of the male and female molds to reduce the pressure holding, etc. The adjustment of small parts deformation mainly depends on the pressure. The adjustment of mold temperature, time and deformation of large parts generally relies on mold temperature.


11. Unclean surface

This is due to the rough surface of the mold.

☞ Improvement method: For PC materials, sometimes due to the mold temperature being too high, there are residual glue and oil stains on the mold surface. The mold surface needs to be cleaned, polished, and the mold temperature reduced in time.


12. Pull white

It easily occurs at the thin-walled corners of molded products or at the roots of thin-walled RIBs. It is caused by poor stress during demoulding, improper ejection pin setting or insufficient draft angle.

☞ Improvement methods: increase the R angle at the corner, increase the demoulding angle, increase the ejector pin or increase its cross-sectional area, polish the mold surface, polish the ejector pin or oblique pin, reduce the shooting speed, reduce the injection pressure, and reduce the maintenance Pressure and time, etc.


13. Die drawing

It manifests itself as poor demolding, mold damage, or embossing. Mainly due to insufficient draft angle or rough mold surface, the molding conditions also have an impact.

☞ Improvement methods: increase the draft angle, polish the mold surface, add or change the pull pin when gluing the female mold surface, pay attention to the horn diameter when feeding horns, add nip to the male mold, reduce the injection pressure, and reduce the holding pressure and time etc.


14. Stomata

Transparent finished PC materials are prone to appear during molding. Since the gas is not exhausted during the injection molding process, improper mold design or improper molding conditions will have an impact.

☞ Improvement methods: increase exhaust, change the gate (increase the inlet gate), PC material flow channel must be polished, strict baking conditions, increase injection pressure, reduce injection speed, etc.


15. Breakage

It occurs at the joints of male and female modules, sliders, oblique pins, etc. It is manifested as uneven levels of the joint surface, etc., due to improper mold closing or problems with the mold itself.

☞ Improvement method: Correct the mold, or re-close the mold.


16. Dimensions out of tolerance

 


Problems with the mold itself, or improper molding conditions causing inappropriate molding shrinkage.

☞ Improvement method: Usually changing the holding time and injection pressure (second paragraph) have the greatest impact on the size. For example: increasing the injection pressure, increasing the pressure-holding and shrinkage effect can significantly increase the size, lowering the mold temperature can also be used, and increasing the gate or increasing the gate can improve the adjustment effect.

 

 

Send Inquiry

whatsapp

skype

E-mail

Inquiry