1. If the size of any product reaches 200mm or more, the inner edge of the exhaust groove of the product is preferably 10-15mm away from the outer edge of the product, and the contact surface of the parting line is 30-50mm or more, as shown in the figure below. Be careful when avoiding the air Note the runner.
This product has a length of 255mm
Leave 25-30mm for the parting surface of the product
Leave 10mm on the edge of the model, and avoid the green part by 0.15mm
Pay attention to the sharp corner rounding of the empty part
2. For products with a size of 100-200mm, it is better for the inner edge of the exhaust groove to be 8-10mm away from the outer edge of the product, and the parting contact surface is 30-40mm or more.
This product has 124mm length
Leave 20-25mm for the parting surface of the product
Leave 10mm on the edge of the model, and avoid the red part
Pay attention to the sharp corner rounding of the empty part
3. For products below 100, it is better for the inner edge of the exhaust groove to be 6-8mm away from the outer edge of the product, and the parting contact surface is 20-30mm or more.
This product is 52mm long
Leave 15-20mm for the parting surface of the product
Leave 10mm on the edge of the model, and avoid the pink part by 0.15mm
Pay attention to the sharp corner rounding of the empty part
4. AB molding class, as shown in the figure below.
Leave 30-50mm for the parting surface of the product
5. Avoidance of the special-shaped parting surface, as shown in the figure below.
The parting surface of the mold is relatively irregular, and the height difference is relatively large
These only need to leave 25mm glue points, and the back can be avoided
6. There is a puncture position for this product. If the area is relatively large, leave 10-15mm at the edge, and avoid 0.15mm in the middle red, so that it is convenient for the fitter to make molds.
In plastic mold design, avoiding space (also called relieving or relieving the parting line / 避空) refers to stepping back non-contact areas of the core and cavity steel so that fitting pressure concentrates strictly on the sealing shut-offs.
When you notice a "thick middle, thin edges" phenomenon on the molded part or the mold steel after adding relief, it is usually a sign of steel deflection, clamping force imbalance, or thermal expansion.
UNRELIEVED / IMPROPER RELIEF PROPER PARTING LINE RELIEF ┌──────────────────────────────────┐ ┌──────────────────────────────────┐ │ TOP MOLD CORE │ │ TOP MOLD CORE │ ├──────────────────────────────────┤ ├──────┐ ┌──────┤ │░░░░░░░░░░░ CAVITY ░░░░░░░░░░░░░░░│ │░░░░░░│ CAVITY │░░░░░░│ ├──────────────────────────────────┤ ├──────┘ └──────┤ │ BOTTOM MOLD CAVITY │ │ BOTTOM MOLD CAVITY │ └──────────────────────────────────┘ └──────────────────────────────────┘ Pressure spreads out everywhere Pressure concentrates on sealing land
Why Does the "Thick Middle, Thin Edges" Defect Happen?
1. Mold Center Deflection (Bowing Under Injection Pressure)
When high plastic injection pressure enters the cavity, it exerts tons of outward force against the mold cores.
If the relief around the outer perimeter of the mold is too large or too close to the cavity, the core steel lacks support in the middle.
Under 1,000+ bar injection pressure, the mold core flexes or bows outward at the center, making the plastic wall thicker in the middle and thinner at the clamped outer edges.
2. Excessive Clamping Pressure Distorting the Outer Sealing Lands
If the relieved area in the center is cut too deep or wide, the entire clamping tonnage of the injection molding machine concentrates on a small outer "land area" (shut-off margin).
This extreme tonnage crushes the outer steel edges over time.
As the outer shut-off lands compress and deform, the mold plates pinch tighter at the perimeter while leaving a larger gap (thicker section) in the center.
3. Uneven Thermal Expansion (Hot Center, Cool Edges)
Mold cores run much hotter near the center gates where hot plastic continuously enters.
The center of the mold steel expands thermally more than the cooled outer perimeter.
If the parting surface relief doesn't account for thermal expansion gradients, the thermal crowning forces the center open slightly during high-speed production, yielding a thicker wall in the middle.
4. Improper Shut-Off Land Width Selection
When designing parting surface relief, engineers must balance shut-off contact area with relieved clearance:
| Metric | Too Small / Too Narrow | Optimal Range | Too Large / Too Deep |
| Shut-Off Land Width | Steel crushes under clamping tonnage; causes thin edges | 15 mm – 30 mm (depending on mold size) | Clamping force dilutes; causes flash across parting line |
| Relief Depth | No effect (steel still touches) | 0.5 mm – 1.0 mm | Reduces core backing support, leading to center flex |
How to Correct Parting Line Relief Problems
Check Machine Clamping Force: Reduce machine clamping tonnage to prevent crushing the outer non-relieved shut-off lands.
Add Pillar Supports (Support Pins): Install heavy-duty support pillars (Ejector Housing Support Pins / 撑头) directly underneath the center of the cavity/core insert to prevent center deflection under injection pressure.
Verify Shut-Off Land Dimensions: Ensure the contact land around the cavity perimeter is at least 15–25 mm wide. Do not relieve steel too close to the cavity edge.
Inspect Steel Blue Matching (Spotting): Perform a red lead / Prussian blue spotting test on the bench to verify that contact pressure is evenly distributed across both the center and outer shut-off surfaces.